In this paper, the research process of the fire - proof calcium silicate board trial - produced with theindustrial tailings - felspar powder is reported.
For sinter with 25% and 50% MAC fines the iron oxides mainly consisted of hematite and magnetite, the bonding phase were mainly dicalcium silicate, glassiness, and a few amount of calcium ferrite.
Temperatures on this planet can get higher than 900 degrees Celsius, which heats the silicate particles in the atmosphere, potentially giving rise to molten glass rain.
Using the serial analysis method, researchers obtained space weathering information of silicates, oxides, phosphates and sulfides on the surface of a single particle of lunar soil collected by Chang'e-5.